TPU 95A Settings for Voxelab Aquila X2

Recommended slicer settings for printing TPU 95A on the Voxelab Aquila X2 (220 x 220 x 250 mm build volume, 180 mm/s max speed, Bowden extruder).

根据厂商规格计算intermediate

切片配置

将这些参数复制到你的切片软件(Cura、OrcaSlicer、PrusaSlicer、Bambu Studio)
参数数值范围
喷嘴温度223°C210-235°C
热床温度50°C40-60°C
首层喷嘴228°C+5°C above normal
首层热床55°C+5°C above normal
打印速度23 mm/s15-30 mm/s
首层速度15 mm/s25-50% of normal
外壁速度17 mm/s70-80% of normal
空走速度45 mm/s120-150% of print speed
层高0.2mm0.12-0.28mm
Infill15-20%10-30%
壁数3-4Perimeters/shells
顶层/底层5-6Solid layers
散热风扇100%From layer 2+
回抽距离4-6 mmBowden
回抽速度40 mm/sBowden

开始打印前

!
Filament Drying50°C for 5h
EnclosureNot needed
Nozzle TypeStandard brass 0.4mm
ExtruderBowden
Bowden extruder — printing flexible filaments is challenging. Print very slowly and minimize retraction.

打印质量预设

Three presets for common use cases with TPU 95A on the Voxelab Aquila X2.

ProfileLayer HeightSpeedInfillBest For
Draft0.28mm30 mm/s10-15%Rapid prototyping, test fits
Standard0.20mm23 mm/s15-20%General purpose, everyday prints
Quality0.12mm15 mm/s20-30%Miniatures, display pieces, fine detail

热床附着

TPU 95A(Shore 95A)粘合良好到大多数表面,包括 PEI 片、蓝色美纹纸和带胶棒的玻璃。粘合很少是问题 -- 灵活性帮助它抓住热床。

温度调校指南

Nozzle: 223°C

Range: 210-235°C. Printer max: 260°C.

  • Poor layer adhesion? Increase +5°C
  • Stringing or oozing? Decrease -5°C
  • Print a temperature tower to find your exact sweet spot

Bed: 50°C

Range: 40-60°C. Printer max: 100°C.

  • First layer lifting? Increase +5°C
  • Elephant's foot? Decrease -5°C
  • Let the bed fully preheat before starting

在 Voxelab Aquila X2 上打印 TPU 95A 的问题排查

耗材卡顿打印缓慢(20-40 mm/s);检查挤出机路径中耗材可能屈曲的间隙
拉丝降低温度、提高行程速度并使用最小回抽(直接驱动 0.5-1mm)
挤出不足增加流量 5-10% 并进一步降低打印速度
研磨减少回抽距离并检查挤出机齿轮张力 -- 对柔性耗材更少更好

TPU 95A 使用技巧

1

Shore 95A 是最常见且最容易打印的 TPU -- 如果是柔性耗材新手,从这里开始

2

速度是一切:最多 20-40 mm/s,对于复杂几何更慢

3

最小化回抽(直接驱动 0.5-1mm) -- 过度回抽卡顿柔性耗材

4

在湿度大的气候下干燥后使用;TPU 是吸水性的

支撑设置

For prints requiring supports with TPU 95A, use tree supports for easier removal and less scarring. Set a 0.15-0.2mm Z-distance between support and model. If you have a dual-extruder setup, consider PVA (for PLA/PETG) or HIPS (for ABS) as dedicated water/solvent-soluble support material.

Voxelab Aquila X2 Specs

Build Volume220 x 220 x 250 mm
Max Speed180 mm/s
Max Nozzle Temp260°C
Max Bed Temp100°C
ExtruderBowden

TPU 95A Properties

Nozzle Range210-235°C
Bed Range40-60°C
Speed Range15-30 mm/s
Difficultyintermediate
Drying50°C / 5h
EnclosureNot needed
了解更多关于 TPU 95A 的信息 →

TPU 95A 速览

优势

  • Standard flexible filament — Shore 95A hardness
  • Good balance of flexibility and printability
  • Excellent impact and abrasion resistance
  • Stretches 300-500% before breaking

劣势

  • Must print slowly
  • Difficult on Bowden extruders — direct drive preferred
  • Minimal retraction needed (causes jams)
  • Stringing is common
这些参数是基于厂商规格和社区经验的推荐起点。请先做测试打印并按需调整。具体参数可能会因你的打印机状态、环境和耗材批次而有所不同。

想要个性化的 AI 参数?

描述你的具体配置和要打印的内容。3DSearch 的 AI 专家会在几秒内为你的 Voxelab Aquila X2 搭配 TPU 95A 生成定制切片参数。

试用 3DSearch →

来源: Based on manufacturer specifications and community recommendations, community testing data, manufacturer recommended ranges. 参数根据耗材规格和打印机硬件上限计算得出。