Nylon Settings for Voxelab Aquila X2
Recommended slicer settings for printing Nylon on the Voxelab Aquila X2 (220 x 220 x 250 mm build volume, 180 mm/s max speed, Bowden extruder).
Slicer Configuration
Copy these values into your slicer (Cura, OrcaSlicer, PrusaSlicer, Bambu Studio)| Setting | Value | Range |
|---|---|---|
| Nozzle Temperature | 260°C | 240-280°C |
| Bed Temperature | 80°C | 70-90°C |
| First Layer Nozzle | 260°C | At printer max |
| First Layer Bed | 85°C | +5°C above normal |
| Print Speed | 40 mm/s | 30-50 mm/s |
| First Layer Speed | 15 mm/s | 25-50% of normal |
| Wall Speed | 30 mm/s | 70-80% of normal |
| Travel Speed | 75 mm/s | 120-150% of print speed |
| Layer Height | 0.2mm | 0.12-0.28mm |
| Infill | 15-20% | 10-30% |
| Wall Count | 2-3 | Perimeters/shells |
| Top/Bottom Layers | 3-4 | Solid layers |
| Cooling Fan | 0-10% | From layer 2+ |
| Retraction Distance | 4-6 mm | Bowden |
| Retraction Speed | 40 mm/s | Bowden |
Before You Print
Print Quality Profiles
Three presets for common use cases with Nylon on the Voxelab Aquila X2.
| Profile | Layer Height | Speed | Infill | Best For |
|---|---|---|---|---|
| Draft | 0.28mm | 50 mm/s | 10-15% | Rapid prototyping, test fits |
| Standard | 0.20mm | 40 mm/s | 15-20% | General purpose, everyday prints |
| Quality | 0.12mm | 30 mm/s | 20-30% | Miniatures, display pieces, fine detail |
Bed Adhesion
Nylon is notoriously difficult for bed adhesion. Use a PEI sheet with glue stick, or a Garolite (G10) sheet for the best results. A brim is essential for most nylon prints. Some users also find blue painter's tape with glue stick works well.
Temperature Tuning Guide
Nozzle: 260°C
Range: 240-280°C. Printer max: 260°C.
- Poor layer adhesion? Increase +5°C
- Stringing or oozing? Decrease -5°C
- Print a temperature tower to find your exact sweet spot
Bed: 80°C
Range: 70-90°C. Printer max: 100°C.
- First layer lifting? Increase +5°C
- Elephant's foot? Decrease -5°C
- Let the bed fully preheat before starting
Troubleshooting Nylon on Voxelab Aquila X2
Pro Tips for Nylon
Drying is absolutely critical -- even new sealed spools benefit from 12+ hours of drying at 80°C
Print from a dry box or active filament dryer; nylon re-absorbs moisture during the print
Garolite (G10) sheets provide the best bed adhesion for nylon
After printing, you can boil nylon parts to moisture-condition them -- this triples impact strength
Start with PA12 if you are new to nylon; it is much easier to print than PA6
Support Settings
For prints requiring supports with Nylon, use tree supports for easier removal and less scarring. Set a 0.15-0.2mm Z-distance between support and model. If you have a dual-extruder setup, consider PVA (for PLA/PETG) or HIPS (for ABS) as dedicated water/solvent-soluble support material.
Voxelab Aquila X2 Specs
| Build Volume | 220 x 220 x 250 mm |
| Max Speed | 180 mm/s |
| Max Nozzle Temp | 260°C |
| Max Bed Temp | 100°C |
| Extruder | Bowden |
Nylon Properties
| Nozzle Range | 240-280°C |
| Bed Range | 70-90°C |
| Speed Range | 30-50 mm/s |
| Difficulty | advanced |
| Drying | 80°C / 16h |
| Enclosure | Recommended |
Nylon at a Glance
Strengths
- Highest tensile strength among common filaments (50-90 MPa)
- Excellent wear and abrasion resistance
- Excellent fatigue resistance (living hinges, snap fits)
- Good heat resistance (PA6 softens ~180C)
- Ideal for gears, bearings, and mechanical parts
Weaknesses
- Extremely hygroscopic (absorbs moisture rapidly)
- Requires extensive drying (12-20 hours)
- Must print from a dry box
- Warps aggressively without enclosure
- Difficult to get right for beginners
Want personalized AI settings?
Describe your exact setup and what you are printing. 3DSearch's AI expert generates custom slicer settings for your Voxelab Aquila X2 with Nylon in seconds.
Try 3DSearch →Sources: Based on manufacturer specifications and community recommendations, community testing data, manufacturer recommended ranges. Values calculated from filament specifications and printer hardware limits.