TPU 95A Settings for Markforged Onyx Pro
Recommended slicer settings for printing TPU 95A on the Markforged Onyx Pro (320 x 132 x 154 mm build volume, 200 mm/s max speed, direct drive extruder).
Niet compatibelintermediate
Niet compatibel
The max bed temperature of 0°C is below the recommended 40°C for TPU 95A. Adhesion may be poor without additional bed adhesion aids.
| Filament Nozzle Requirement | 210-235°C |
| Printer Max Nozzle | 280°C |
| Filament Bed Requirement | 40-60°C |
| Printer Max Bed | N/A |
Wat je in plaats daarvan kunt doen
- Your printer's bed maxes out at 0°C, but TPU 95A needs at least 40°C for reliable adhesion.
- Try a compatible filament for your Markforged Onyx Pro — PLA, PETG, and ABS are good options.
- If you need TPU 95A specifically, you'll need a printer with a hotend capable of 210°C+ nozzle.
TPU 95A Requirements
TPU 95A Properties
| Nozzle Range | 210-235°C |
| Bed Range | 40-60°C |
| Speed Range | 15-30 mm/s |
| Difficulty | intermediate |
| Enclosure | Not needed |
| Drying | 50°C / 5h |
Markforged Onyx Pro Specs
| Build Volume | 320 x 132 x 154 mm |
| Max Speed | 200 mm/s |
| Max Nozzle Temp | 280°C |
| Max Bed Temp | N/A |
| Extruder | Direct Drive |
TPU 95A in één oogopslag
Sterke punten
- Standard flexible filament — Shore 95A hardness
- Good balance of flexibility and printability
- Excellent impact and abrasion resistance
- Stretches 300-500% before breaking
Zwakke punten
- Must print slowly
- Difficult on Bowden extruders — direct drive preferred
- Minimal retraction needed (causes jams)
- Stringing is common
Wil je gepersonaliseerde AI-instellingen?
Beschrijf je exacte setup en wat je afdrukt. 3DSearch's AI-expert genereert in seconden aangepaste slicer-instellingen voor je Markforged Onyx Pro met TPU 95A.
Probeer 3DSearch →Bronnen: Based on manufacturer specifications and community recommendations, community testing data, manufacturer recommended ranges. Waarden berekend op basis van filamentspecificaties en printerhard warelimiet.