TPU Settings for Prusa Core One

Recommended slicer settings for printing TPU on the Prusa Core One (250 x 220 x 270 mm build volume, 500 mm/s max speed, direct drive extruder).

إعدادات موثقةintermediate

إعدادات Slicer

انسخ هذه القيم إلى Slicer الخاص بك (Cura, OrcaSlicer, PrusaSlicer, Bambu Studio)
الإعدادالقيمةالنطاق
درجة حرارة الفوهة225°C210-240°C
درجة حرارة المنصة50°C40-60°C
الفوهة للطبقة الأولى230°C+5°C above normal
المنصة للطبقة الأولى55°C+5°C above normal
سرعة الطباعة30 mm/s20-40 mm/s
سرعة الطبقة الأولى15 mm/s25-50% of normal
سرعة الجدران23 mm/s70-80% of normal
سرعة الانتقال60 mm/s120-150% of print speed
ارتفاع الطبقة0.2mm0.12-0.28mm
Infill15-20%10-30%
عدد الجدران3-4Perimeters/shells
الطبقات العلوية/السفلية5-6Solid layers
مروحة التبريد100%From layer 2+
مسافة السحب0.5-1.0 mmDirect drive
سرعة السحب25 mm/sDirect drive

قبل أن تطبع

!
Filament Drying70°C for 7h
EnclosureNot needed
Nozzle TypeStandard brass 0.4mm
ExtruderDirect Drive
Direct drive — well suited for flexible filaments.

ملفات تعريف جودة الطباعة

Three presets for common use cases with TPU on the Prusa Core One.

ProfileLayer HeightSpeedInfillBest For
Draft0.28mm40 mm/s10-15%Rapid prototyping, test fits
Standard0.20mm30 mm/s15-20%General purpose, everyday prints
Quality0.12mm20 mm/s20-30%Miniatures, display pieces, fine detail

التصاق بالمنصة

TPU adheres well to most surfaces including PEI sheets, blue painter's tape, and glass with glue stick. Adhesion is rarely an issue with TPU.

دليل ضبط درجة الحرارة

Nozzle: 225°C

Range: 210-240°C. Printer max: 290°C.

  • Poor layer adhesion? Increase +5°C
  • Stringing or oozing? Decrease -5°C
  • Print a temperature tower to find your exact sweet spot

Bed: 50°C

Range: 40-60°C. Printer max: 120°C.

  • First layer lifting? Increase +5°C
  • Elephant's foot? Decrease -5°C
  • Let the bed fully preheat before starting

استكشاف أخطاء TPU على Prusa Core One

Filament jammingReduce print speed significantly; check extruder path for gaps where flexible filament can buckle
StringingReduce temperature, increase travel speed, and reduce retraction distance (less is more with TPU)
Under-extrusionIncrease flow rate by 5-10% and slow down the print speed
Grinding filamentReduce retraction distance and check extruder gear tension

نصائح احترافية لـ TPU

1

Speed is the most critical setting -- printing too fast is the number one cause of TPU failures

2

A direct drive extruder is strongly recommended; Bowden setups struggle with flexible filaments

3

Minimize retraction (0.5-1mm on direct drive) -- excessive retraction causes jams

4

Dry your TPU before every use in humid climates; it is very hygroscopic

5

Consider starting with Shore 95A TPU -- it is the easiest flexible filament to print

إعدادات الدعائم

For prints requiring supports with TPU, use tree supports for easier removal and less scarring. Set a 0.15-0.2mm Z-distance between support and model. If you have a dual-extruder setup, consider PVA (for PLA/PETG) or HIPS (for ABS) as dedicated water/solvent-soluble support material.

Prusa Core One Specs

Build Volume250 x 220 x 270 mm
Max Speed500 mm/s
Max Nozzle Temp290°C
Max Bed Temp120°C
ExtruderDirect Drive

TPU Properties

Nozzle Range210-240°C
Bed Range40-60°C
Speed Range20-50 mm/s
Difficultyintermediate
Drying70°C / 7h
EnclosureNot needed
اعرف المزيد عن TPU →

TPU في لمحة

نقاط القوة

  • Flexible and rubber-like
  • Excellent impact absorption
  • Excellent abrasion resistance
  • 300-600% elongation at break
  • Great for phone cases, gaskets, wheels, dampeners

نقاط الضعف

  • Must print very slowly
  • Difficult on Bowden extruders
  • High moisture sensitivity
  • Stringing is common
  • Retraction must be minimized
هذه الإعدادات هي نقاط بداية موصى بها استنادًا إلى مواصفات الشركة المصنعة وإرشادات المجتمع. قم دائمًا بطباعة تجريبية واضبط حسب الحاجة. قد تختلف الإعدادات حسب حالة طابعتك المحددة والبيئة ودفعة الفيلامنت.

تريد إعدادات AI مخصصة؟

صِف إعدادك الدقيق وما تطبعه. يُنشئ خبير AI في 3DSearch إعدادات تقطيع مخصصة لطابعتك Prusa Core One مع TPU خلال ثوانٍ.

جرّب 3DSearch →

المصادر: Based on Prusa Knowledge Base (help.prusa3d.com), community testing data, manufacturer recommended ranges. تم التحقق من القيم من وثائق الشركة المصنعة وملفات التقطيع الرسمية.