BVOH Settings for Markforged X7

Recommended slicer settings for printing BVOH on the Markforged X7 (330 x 270 x 200 mm build volume, 200 mm/s max speed, direct drive extruder).

Uyumlu Değilbeginner

Uyumlu Değil

The max bed temperature of 0°C is below the recommended 50°C for BVOH. Adhesion may be poor without additional bed adhesion aids.

Filament Nozzle Requirement190-220°C
Printer Max Nozzle300°C
Filament Bed Requirement50-60°C
Printer Max BedN/A

Bunun yerine yapılması gerekenler

  • Your printer's bed maxes out at 0°C, but BVOH needs at least 50°C for reliable adhesion.
  • Try a compatible filament for your Markforged X7 — PLA, PETG, and ABS are good options.
  • If you need BVOH specifically, you'll need a printer with a hotend capable of 190°C+ nozzle.

BVOH Requirements

BVOH Properties

Nozzle Range190-220°C
Bed Range50-60°C
Speed Range20-40 mm/s
Difficultybeginner
EnclosureNot needed
DryingNot required

Markforged X7 Specs

Build Volume330 x 270 x 200 mm
Max Speed200 mm/s
Max Nozzle Temp300°C
Max Bed TempN/A
ExtruderDirect Drive

BVOH Bir Bakışta

Güçlü Yönleri

  • Water-soluble support material
  • Dissolves faster than PVA (2-4 hours)
  • Works with wider range of build materials
  • Leaves very clean supported surfaces

Zayıf Yönleri

  • Extremely moisture sensitive — use immediately after opening
  • More expensive than PVA
  • Must store in sealed dry container
  • Limited shelf life once opened

Kişiselleştirilmiş yapay zeka ayarları ister misin?

Tam kurulumunu ve ne yazdırdığını açıkla. 3DSearch'ün yapay zeka uzmanı saniyeler içinde BVOH ile Markforged X7 için özel slicer ayarları oluşturuyor.

3DSearch'ü dene →

Kaynaklar: Based on manufacturer specifications and community recommendations, community testing data, manufacturer recommended ranges. Değerler filament belirtimleri ve yazıcı donanım sınırlarından hesaplanmıştır.