TPU Settings for Voron 0.2
Recommended slicer settings for printing TPU on the Voron 0.2 (120 x 120 x 120 mm build volume, 300 mm/s max speed, direct drive extruder).
Quick Reference
Temperature Settings
Start with the nozzle at 225°C and the bed at 50°C. If you see poor layer adhesion, increase the nozzle temperature by 5°C increments. If you experience stringing, decrease the nozzle temperature by 5°C. For the first layer, you can increase the bed temperature by 5°C for better adhesion, then let it drop back to 50°C for subsequent layers.
The TPU filament has a recommended nozzle temperature range of 210-240°C and a bed temperature range of 40-60°C. The Voron 0.2 supports nozzle temperatures up to 300°C and bed temperatures up to 110°C, which fully covers the recommended range for this filament.
Speed & Quality
The Voron 0.2 supports high-speed printing at up to 300 mm/s. For TPU, we recommend 20-50 mm/s for general printing. Start with the lower end for quality-critical prints and increase for draft prints. Always print the first layer at 25-50% of your normal speed for better adhesion.
For quality-critical prints like miniatures or display pieces, reduce the speed to 20 mm/s and use a 0.12-0.16mm layer height. For draft or rapid prototyping, you can push the speed to 50 mm/s with a 0.24-0.28mm layer height. The standard 0.2mm layer height at 35 mm/s provides the best balance of speed and quality for most prints.
Bed Adhesion
TPU adheres well to most surfaces including PEI sheets, blue painter's tape, and glass with glue stick. Adhesion is rarely an issue with TPU.
Common Issues with TPU on Voron 0.2
Here are the most common problems you may encounter when printing TPU on the Voron 0.2, along with proven solutions:
- Filament jamming: Reduce print speed significantly; check extruder path for gaps where flexible filament can buckle
- Stringing: Reduce temperature, increase travel speed, and reduce retraction distance (less is more with TPU)
- Under-extrusion: Increase flow rate by 5-10% and slow down the print speed
- Grinding filament: Reduce retraction distance and check extruder gear tension
Tips for Best Results
Follow these expert tips to get the best possible prints with TPU on your Voron 0.2:
- Speed is the most critical setting -- printing too fast is the number one cause of TPU failures
- A direct drive extruder is strongly recommended; Bowden setups struggle with flexible filaments
- Minimize retraction (0.5-1mm on direct drive) -- excessive retraction causes jams
- Dry your TPU before every use in humid climates; it is very hygroscopic
- Consider starting with Shore 95A TPU -- it is the easiest flexible filament to print
Support Settings
For prints requiring supports with TPU, use tree supports for easier removal and less scarring. Set a 0.15-0.2mm Z-distance between support and model. If you have a dual-extruder setup, consider PVA (for PLA/PETG) or HIPS (for ABS) as dedicated water/solvent-soluble support material.
TPU at a Glance
Strengths
- Flexible and rubber-like
- Excellent impact absorption
- Excellent abrasion resistance
- 300-600% elongation at break
- Great for phone cases, gaskets, wheels, dampeners
Weaknesses
- Must print very slowly
- Difficult on Bowden extruders
- High moisture sensitivity
- Stringing is common
- Retraction must be minimized
Voron 0.2 Specifications
The Voron 0.2 features a 120 x 120 x 120 mm build volume with a maximum print speed of 300 mm/s. It uses a direct drive extruder system, which provides better control over flexible and specialty filaments. The hotend can reach 300°C and the heated bed supports temperatures up to 110°C.
Want personalized AI settings?
Describe your exact setup and what you are printing. 3DSearch's AI expert generates custom slicer settings for your Voron 0.2 with TPU in seconds.
Try 3DSearch →Sources: Based on manufacturer specifications and community recommendations, community testing data, manufacturer recommended ranges.