ASA Settings for Longer LK5 Pro

Recommended slicer settings for printing ASA on the Longer LK5 Pro (300 x 300 x 400 mm build volume, 180 mm/s max speed, Bowden extruder).

These settings are recommended starting points based on manufacturer specifications and community guidelines. Always do a test print and adjust as needed. Settings may vary based on your specific printer's condition, environment, and filament batch.

Quick Reference

Nozzle Temperature250°C
Bed Temperature100°C
Print Speed40-60 mm/s
Layer Height0.2mm (recommended)
Infill15-20%
Cooling Fan0-10%
Retraction4-6 mm at 40 mm/s
Difficultyintermediate
Enclosure recommended for ASA printing.
Dry filament before use: 77°C for 4 hours.

Temperature Settings

Start with the nozzle at 250°C and the bed at 100°C. If you see poor layer adhesion, increase the nozzle temperature by 5°C increments. If you experience stringing, decrease the nozzle temperature by 5°C. For the first layer, you can increase the bed temperature by 5°C for better adhesion, then let it drop back to 100°C for subsequent layers.

The ASA filament has a recommended nozzle temperature range of 240-260°C and a bed temperature range of 90-110°C. The Longer LK5 Pro supports nozzle temperatures up to 260°C and bed temperatures up to 110°C, which fully covers the recommended range for this filament.

Speed & Quality

For the Longer LK5 Pro, a print speed of 40-60 mm/s works well with ASA. The first layer should be printed at 15-25 mm/s for solid bed adhesion. Outer walls at 70-80% of the main speed produce cleaner surface finishes.

For quality-critical prints like miniatures or display pieces, reduce the speed to 40 mm/s and use a 0.12-0.16mm layer height. For draft or rapid prototyping, you can push the speed to 60 mm/s with a 0.24-0.28mm layer height. The standard 0.2mm layer height at 50 mm/s provides the best balance of speed and quality for most prints.

Bed Adhesion

ASA uses the same bed adhesion methods as ABS: PEI sheet at high temperature, glue stick, or ASA/ABS slurry. A brim is recommended for larger parts to prevent warping.

Common Issues with ASA on Longer LK5 Pro

Here are the most common problems you may encounter when printing ASA on the Longer LK5 Pro, along with proven solutions:

Tips for Best Results

Follow these expert tips to get the best possible prints with ASA on your Longer LK5 Pro:

Support Settings

For prints requiring supports with ASA, use tree supports for easier removal and less scarring. Set a 0.15-0.2mm Z-distance between support and model. If you have a dual-extruder setup, consider PVA (for PLA/PETG) or HIPS (for ABS) as dedicated water/solvent-soluble support material.

ASA at a Glance

Strengths

  • Best UV resistance of common filaments (10x better than ABS)
  • Excellent for outdoor functional parts
  • Does not yellow or become brittle in sunlight
  • Good impact resistance (similar to ABS)
  • Good heat resistance (softens ~100C)

Weaknesses

  • Requires enclosure (like ABS)
  • Emits fumes (similar to ABS)
  • More expensive than ABS
  • Still prone to warping without enclosure

Longer LK5 Pro Specifications

The Longer LK5 Pro features a 300 x 300 x 400 mm build volume with a maximum print speed of 180 mm/s. It uses a Bowden extruder system, which is lighter on the print head but may require additional tuning for flexible filaments like TPU. The hotend can reach 260°C and the heated bed supports temperatures up to 110°C.

Want personalized AI settings?

Describe your exact setup and what you are printing. 3DSearch's AI expert generates custom slicer settings for your Longer LK5 Pro with ASA in seconds.

Try 3DSearch →

Sources: Based on manufacturer specifications and community recommendations, community testing data, manufacturer recommended ranges.